Published in Extreme Mechanics Letters, 2021
Recommended citation: K. Ding#, Y. Zhang#, A. Birnbaum, J. Michopoulos, D. McDowell, T. Zhu*, "Strain gradient plasticity modeling of nanoindentation of additively manufactured stainless steel." Extreme Mechanics Letters, 49, 101503 (2021). https://www.sciencedirect.com/science/article/pii/S2352431621001954